Assessing the pH and DP of canvasses with NIR spectroscopy

Data de publicació

2013-11-05T12:21:09Z

2013-11-05T12:21:09Z

2013-11

Resum

Podeu consultar el document complet a: http://hdl.handle.net/2445/47384


The canvas support in easel paintings is composed mainly of cellulose. One of the main degradation paths of cellulose is acid-catalysed hydrolysis, which means that in an acidic environment (low pH), its degradation proceeds at a faster rate (Strlič et al., 2005). The main effect of acid-catalysed hydrolysis is the breaking up of the polymer chains, measured by the “Degree of Polymerisation” (DP). The lowering of the DP value implies a lower mechanical strength of the textile (Scicolone, 1993), and thus this parameter can be used to monitor degradation. Knowing these two parameters can, therefore, be very informative regarding the condition of the canvas support.

Tipus de document

Objecte de conferència

Llengua

Anglès

Publicat per

Universitat de Barcelona. Facultat de Belles Arts. Secció de Conservació-Restauració

Documents relacionats

Comunicació presentada a: La Recerca en Conservació des de la Visió del Conservador-Restaurador. Setmana de la Ciència, Barcelona, 7 i 8 de novembre de 2013, ISBN: 13:978-84-695-885-7, p. 79-87

http://hdl.handle.net/2445/47384

Citació recomanada

Aquesta citació s'ha generat automàticament.

Drets

cc-by-nc-nd, (c) Oriola Folch, 2013

http://creativecommons.org/licenses/by-nc-nd/3.0/es/

Aquest element apareix en la col·lecció o col·leccions següent(s)